Diamond Dotted DMD Flexible Laminated Insulating Paper Composite Material
Main Parameters:
Coils: Standard width 1000 mm
Strips: Minimum slit width 4 mm
Sheets: Width and length can be customized
The material can be bonded through a secondary heat-curing process and offers excellent mechanical, dielectric, and adhesive properties.
Diamond Dotted DMD Flexible Laminated Insulating Paper Composite Material Description
Dotted-adhesive DMD is a flexible composite insulating material consisting of a Class F polyester film and a polyester non-woven fabric, with a special diamond-patterned epoxy adhesive applied to the surface and cured to a B-stage. The material can be bonded through a secondary heat-curing process and offers excellent mechanical, dielectric, and adhesive properties.
Diamond Dotted DMD Flexible Laminated Insulating Paper Composite Material Technical
| Item | Unit | Value | |||||||
| Base material thickness | mm | 0.1 | 0.13 | 0.15 | 0.17 | 0.2 | 0.25 | 0.3 | |
| Limit deviation of thickness | mm | ±0.02 | ±0.03 | ||||||
| Thickness of single-sided adhesive | um | 5-15 | |||||||
| Contamination of transformer oil | / | Pollution-free(△tans<0.001) | |||||||
| Tensile strength without bending | longitudinal | N/10mm | 60 | 90 | ≥100 | ≥120 | ≥140 | ≥190 | ≥270 |
| Horizontal | 50 | 80 | ≥90 | ≥105 | ≥120 | ≥170 | ≥200 | ||
| Elongation at break | longitudinal | % | ≥15 | ||||||
| Horizontal | ≥20 | ||||||||
| Breakdown voltage (normal conditions) | KV | 4 | 5 | 6 | 7 | 9 | 12 | 15 | |
| Long-term heat resistance | / | ≥155 | |||||||
| Curing conditions | Low temperature 90±5℃,2h;high temperature 140±5℃,≥4h | ||||||||
| Bond strength | KPa | ≥350 | |||||||
Get Free Quote of Diamond Dotted DMD Paper
Get competitive price and good quality diamond dotted DMD paper
Diamond Dotted DMD Flexible Laminated Insulating Paper Composite Material Applications
Primarily used for interlayer, interturn, and end insulation in transformers, as well as for wrapping flat copper or aluminum conductors.