Main Parameters:
Modified alkyd quick-drying insulation impregnating varnish is made by modified alkyd resin, ammonia resin, solvent, etc.
| Item | Test condition | Urit | Value | |
| Appearance | – | – | Yellowish-brown liquid, no mechanical impurities | |
| Viscosity | Viscometer No.4, at (23±2) °C | s | 30 〜60 | |
| Drying time | Dry to touch | 23±2°C | Min | <10 |
| Hard Dry | 23±2°C | Hour | <24h | |
| Hard dry | 80°C | Hour | <3h | |
| Specific gravity | 25°C | g/cm3 | 0.93-0.94 | |
| Solid content | 105°C/2h | % | <38 | |
| Power frequency electrical strength | At room temperature | MV/m | >60 | |
| After being humidified | >30 | |||
| Volume resistivity | At room temperature | Q • m | >1×1012 | |
| After being humidified | >1×1010 | |||
| Shelflife | month | 6 | ||